Estimate the theoretical density of an alloy from its composition, using the rule of mixtures. Useful for checking a supplier’s density figure, planning a melt, or working out how much a custom target should weigh.
| Element / component | Weight % | Density (g/cm³) | |
|---|---|---|---|
— g/cm³
Total composition — %
Common alloy densities for reference
| Copper 70 / Zinc 30 (brass) | ≈ 8.39 g/cm³ |
|---|---|
| Copper 90 / Nickel 10 | ≈ 8.95 g/cm³ |
| Gold 80 / Tin 20 (AuSn) | ≈ 14.5 g/cm³ |
| Indium 52 / Tin 48 | ≈ 7.3 g/cm³ |
| Tin 96.5 / Silver 3 / Copper 0.5 (SAC305) | ≈ 7.4 g/cm³ |
The rule of mixtures assumes no volume change on mixing and no porosity. Real cast alloys differ by 1–3% because of intermetallics and shrinkage; sintered or hot-pressed parts differ more, depending on density.