Calculate the mass of material needed to deposit a film of a given thickness over a given area — including the material that never reaches the substrate. This is the number to compare with your crucible charge, not the film mass alone.
— g charge
Film mass — mg · area — cm²
How the calculation works
| Film volume | V = area (cm²) × thickness (cm) |
|---|---|
| Film mass | mfilm = V × density |
| Charge required | mcharge = mfilm ÷ utilisation efficiency |
Utilisation efficiency is the fraction of evaporated material that actually lands on the substrate. Typical values: 20–35% for e-beam with a small source-to-substrate distance, 40–60% for thermal in a close-geometry bell jar, and lower for large chambers or planetary fixtures. If you know your tool’s efficiency from a test run, use that number — it dominates the result far more than density does.