Packaging & Logistics
High-purity metal loses value the moment moisture or oxygen reaches it. Packaging and shipping are part of the specification, not an afterthought — particularly on a 30-day sea crossing.
Packaging by form
| Form | Standard packing | Options |
|---|---|---|
| Ingot / cathode | Strapped bundle, wooden case | VCI film, desiccant, palletised |
| Granule / shot | Argon-flushed vacuum foil bag in drum | 25 / 50 kg drums, moisture-barrier liner |
| Powder | Vacuum-sealed bag, nitrogen-filled drum | Small packs from 1 kg |
| Targets | Individually wrapped, foam-lined crate | Cleanroom bagging on request |
Shipping modes
- Sea freight (LCL/FCL) — bulk tonnage, 25–40 days to US ports
- Air freight — 7–12 days, for urgent or high-value lots
- Express courier — 3–7 days, for samples and small parcels
Incoterms: FOB, CIF, CFR or DDP depending on destination. DDP is available for parcels where duty handling is simpler.
Documents prepared for each shipment
- Commercial invoice with HS codes
- Packing list with lot numbers and net/gross weights
- Certificate of origin
- COA for each lot
- Non-hazardous / non-radioactive declaration, and SDS where required
Reducing risk in transit
For sea freight we add desiccant and VCI protection, and photograph the packing before the container is sealed. If a shipment is delayed, ask for the packing date and whether the drums were opened for inspection — both affect how much moisture the material has seen.