High-purity evaporation materials for e-beam and thermal deposition, from 4N (99.99%) to 6N (99.9999%) for the metals we hold in stock, and up to 7N on request. This page gathers the grades we supply most often, the forms available, and the practical notes that decide whether a run goes well.
Grades we keep in stock
| Aluminium | 4N – 5N5 · pellets, granules · e-beam or thermal |
|---|---|
| Copper | 4N – 6N · pellets, granules, pieces · e-beam |
| Titanium | 2N4 – 4N5 (top grade 4N5) · pellets · e-beam |
| Nickel | 3N5 – 4N5 (standard 4N5) · pellets · e-beam |
| Silver | 4N – 5N · pellets · thermal or e-beam |
| Gold | 4N – 5N · pellets, granules · thermal or e-beam |
| Chromium | 3N – 4N5 · granules, pieces · e-beam |
| Platinum | 3N5 · pellets · e-beam |
| Tin | 4N – 5N · pellets · thermal |
| Tungsten | 3N – 4N · pellets · e-beam |
| Molybdenum | 3N5 – 4N5 · pellets · e-beam |
| Silicon | 4N – 7N · granules · e-beam |
Why the grade depends on the film, not the catalogue
Purity is not a single number. For a metal, the figure that usually decides film quality is the gas content — oxygen, nitrogen, hydrogen — rather than the trace metal total. A 4N5 lot with 800 ppm oxygen will behave worse than a clean 4N lot, and no headline percentage reveals that.
Every certificate we issue states the purity and its basis, the impurity table with detection limits, and the method used. If you are comparing two suppliers, read what 99.99% actually means first.
Forms and what they suit
- Pellets (≈ 3 × 3 mm) — uniform melt level, repeatable fill, best for production runs.
- Granules (1–5 mm) — dense fill, easy to top up mid-run, less bridging.
- Pieces / chunks — lowest cost per kg, uneven first melt.
- Preforms — arc-cast slugs or pressed shapes sized to a specific liner or source.
Choosing between them is covered in e-beam evaporation materials: form, purity and liner.
Packing and certification
Purity-sensitive grades ship vacuum-sealed or argon-flushed, with desiccant where the material is hygroscopic, and a lot label that ties the drum to the assay record. Standard pack is 1 kg per foil bag inside a drum; sample quantities from 100 g. Lead time is 7–15 working days for catalogue grades, 15–25 for custom preforms.
Frequently asked
What is the highest purity you supply?
7N (99.99999%) for silicon; 6N for copper and aluminium; 5N5 for aluminium in stock. Higher grades are quoted against a specific lot.
Do you supply pre-loaded liners?
Yes — material pre-loaded into graphite or boron nitride liners to your source geometry, quoted against the drawing.
Can I get a sample before ordering?
Yes, from 100 g, with the same lot numbering as production so the certificate describes the material you will actually receive.
Related reading: deposition methods compared · purity grades explained · all evaporation materials