Nickel evaporation pellets from Shinray Metals: 3N5 (99.95%) to 4N5 (99.995%), with 4N5 as the standard high-purity grade, supplied as pellets and granules for e-beam evaporation. Nickel is used less for its own film than for what it enables: a diffusion barrier, an adhesion layer, a solderable surface.
Specification
| Metal | Nickel (Ni) |
|---|---|
| Purity | 3N5 (99.95%) – 4N5 (99.995%) · standard high-purity grade 4N5 |
| Form | Pellets ≈ 3 × 3 mm · granules 1–5 mm |
| Density | 8.90 g/cm³ |
| Melting point | 1455 °C |
| Evaporation temperature | ≈ 1600–1800 °C |
| Recommended method | e-beam |
| Packing | Vacuum-sealed foil bag, argon flushed; 1 kg per bag |
| MOQ | 1 kg (samples from 100 g) |
| Lead time | 10–20 working days |
Which grade to order
- 3N5 (99.95%) — decorative coatings, barrier films and general metallisation.
- 4N5 (99.995%) — our standard high-purity grade: barrier and adhesion layers in semiconductor, magnetic film stacks and precision optics.
Iron, cobalt and sulphur are the impurities that matter in nickel — iron and cobalt because they are magnetic and change the film’s behaviour, sulphur because it segregates. Both are in the certificate’s impurity table.
Evaporating nickel
- Magnetic charge. Nickel is ferromagnetic; a long charge can disturb the beam sweep on some sources. Shorter charges or a magnetically compensated source avoid it.
- High temperature, modest rate. Nickel evaporates above 1600 °C; pushing the rate gives a stressed film that later lifts.
- Pre-melt. Nickel picks up sulphur and oxygen on the surface; degassing first avoids a hazy first layer.
- Thin layers are common. 5–50 nm is typical for a barrier or adhesion layer, which means reproducibility matters more than maximum rate.
End applications
- Diffusion barriers and adhesion layers in semiconductor and MEMS
- Seed layers for subsequent plating or soldering
- Magnetic film stacks (with Fe and Co)
- Decorative and corrosion-resistant coatings
- Evaporation feedstock for Ni-based alloys
Frequently asked
Why does my nickel film peel?
Usually stress from a high deposition rate or poor adhesion to the substrate. Slower rate, thinner layer, and a titanium adhesion layer underneath solve most cases.
Can you supply Ni with a stated sulphur content?
Yes — sulphur is reported in the impurity table. For 4N5 we can supply the certificate for the specific lot before shipment.
Related reading: all high-purity evaporation materials · choosing form, purity and liner
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.