Cobalt evaporates at a moderate temperature and is used mainly for magnetic films and as an alloy component. Granules are the practical form for e-beam charges because they fill the liner evenly and can be topped up.
Specification
| Material | Cobalt (Co) |
|---|---|
| Purity | 3N5 – 5N |
| Melting point | 1495 °C |
| Density | 8.90 g/cm³ |
| Form | Pellets, granules or pieces; custom preforms to drawing |
| Packing | Vacuum-sealed, argon flushed; 1 kg per bag |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Evaporation notes
- Ferromagnetic — the charge can disturb the beam sweep on some sources.
- Cobalt oxidises slowly; sealed storage keeps first-melt behaviour repeatable.
- For magnetic stacks, order the same lot as the partner layers.
End applications
- Magnetic film stacks
- Hard and wear-resistant coatings
- Alloy component for CoFe and CoCr
- Battery and catalyst research
Frequently asked
Granules or pellets for cobalt?
Granules fill a liner more densely and are easier to top up mid-run; pellets give a more repeatable melt level.
Is 5N cobalt available?
Yes, up to 5N with a GDASS/ICP certificate, quoted on request.
Related reading: e-beam evaporation materials guide · all high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews