Purity claims are easy to make and hard to check. This page explains exactly how we test, what our certificates contain, and what you can ask for before a lot ships.
1. Sampling
Each production lot is sampled after casting or atomisation, not from the surface of the packaging. For ingot and cathode we take drill or saw chips across the cross-section; for granule and powder we use a rifled splitter to obtain a representative sub-sample. Sample identity is recorded against the lot number before it leaves the plant.
2. Analytical methods
| Method | Measures | Typical use |
|---|---|---|
| ICP-OES | Major and minor metallic impurities (ppm–%) | 3N–4N grades, routine lot release |
| ICP-MS | Trace metals down to ppb | 4N–5N grades, electronics use |
| GDMS | Full trace and ultra-trace survey, including light elements | 5N–6N grades, sputtering targets |
| Inert gas fusion | O, N, H content | Targets and vacuum-melt stock |
All analyses are carried out by accredited third-party laboratories. Our principal partner is Guobiao (Beijing) Testing & Certification Co., Ltd; every certificate names the laboratory that issued the result and the method used, so you always know exactly where each number came from and can audit it independently.
3. What the certificate of analysis (COA) contains
- Lot number and material designation
- Declared purity basis — e.g. “99.99% Cu min, metals basis” (this wording matters)
- Measured impurity elements with values and detection limits
- Analytical method used for each element
- Test date, laboratory name, and approval signature
If a supplier quotes “99.99%” without stating the basis (metals basis vs total, including or excluding oxygen), the number is not comparable. Ask for the impurity table.
4. Traceability
Every drum or bundle carries a lot label: material, purity, form, net weight, lot number and packing date. The lot number links back to the assay record, the raw material batch and the shipment. If you need to qualify a second lot later, we can pull the original data.
5. Packaging
- Ingot / cathode: strapped bundles or wooden cases, VCI film for sea freight
- Granule / powder: argon-flushed, vacuum-sealed foil bags inside steel or fibre drums
- Hygroscopic grades: moisture-barrier liner plus desiccant, sealed under nitrogen
6. Third-party inspection
On request we arrange independent inspection (SGS, BV, CCIC or a lab nominated by the buyer) before shipment. Cost and lead time depend on the scope — tell us at quotation stage.
7. Documents supplied with each shipment
- Certificate of analysis (COA)
- Packing list and commercial invoice
- Certificate of origin
- HS code declaration and, where applicable, non-hazardous / non-radioactive declaration
- Safety data sheet (SDS) on request
Ask for a sample COA with your quotation →
ISO 9001:2015 certification
| Standard | ISO 9001:2015 / GB/T 19001-2016 |
|---|---|
| Certificate number | 04625Q14379R0S |
| Certified organization | Beijing Rotch Technology Co., Ltd. (trading as Shinray Metals) |
| Unified Social Credit Code | 91110109MA01NFYW2F |
| Scope | Sales of Metal Materials, Instruments and Meters, and Non-metallic Mineral Products |
| Issued by | Beijing Head International Certification Co., Ltd. — CNAS C046-M, IAF member |
| Valid | 25 September 2025 – 24 September 2028 |
Certificates are issued to the legal entity; Shinray Metals is the commercial brand used for all quotations, invoices and shipping documents.