Evaporation materials are chosen by process, not only by purity. These are the eight application areas we supply most often, the metals and forms that suit each, and the calculators that size the charge and the film.
Optical coatings
Anti-reflection stacks, mirrors, beam splitters and filters need stable rates, low absorption and reproducible thickness. Silver and aluminium give the highest reflectance; silicon and titanium for high-index layers.
Materials: Silver 4N · Aluminium 4N–5N5 · Silicon 4N–7N · Titanium 2N4–4N5
Display and OLED
Reflectors, cathodes and bus lines. Aluminium is the standard cathode and reflector metal, silver for high-reflectance contacts, copper for conductive bus lines.
Materials: Aluminium · Silver · Copper · Silicon
Semiconductor and MEMS
Contact metallisation, seed layers, electrodes and release layers. Gold and platinum for inert contacts and sensors, aluminium for bond pads, tantalum for diffusion barriers.
Materials: Gold · Platinum · Tantalum · Copper (HP)
Solar and photovoltaic
CIGS back contacts and cell metallisation. Molybdenum is the standard back contact; aluminium, copper and silver for grids; silicon for absorber and passivation work.
Materials: Molybdenum · Aluminium · Copper
Barrier and diffusion layers
Thin dense layers that stop copper or oxygen migration. Tantalum is the classical copper barrier; nickel and chromium for adhesion and corrosion resistance; titanium under gold.
Materials: Tantalum · Nickel · Chromium
Decorative and wear-resistant PVD
Colour, hardness and corrosion resistance on hardware, watch parts and tooling. Titanium and chromium for hard and decorative layers, gold for colour.
Materials: Titanium · Chromium pieces · Gold
High-temperature and aerospace
Films that survive above 1000 °C. Rhenium, tantalum, molybdenum and platinum for sensors, thermocouples and thermal barriers.
Materials: Rhenium · Tantalum · Molybdenum · Platinum
Research and reference films
Small batches for calibration, standards and process development, from 100 g with the same certificate as production lots.
Materials: Gold · Platinum · Cobalt (HP)
Sizing the charge
- Crucible liner fill calculator — usable volume and charge weight for e-beam liners.
- Film material calculator — material needed for a given area and thickness, including utilisation efficiency.