Tantalum evaporates at 3017 °C and is used as a barrier and as a corrosion-resistant layer where aluminium and copper would fail. Because it is a strong getter, the first melt decides film quality more than the purity grade does. Tantalum Evaporation Pellets from Shinray Metals: 3N5 (99.95%) – 4N (99.99%) purity, supplied as pellets (≈ 3 × 3 mm) for e-beam evaporation. Each lot ships with an assay certificate stating the analytical method and detection limits.
Specification
| Metal | Tantalum (Ta) |
|---|---|
| Purity | 3N5 (99.95%) – 4N (99.99%) |
| Form | Pellets — ≈ 3 × 3 mm |
| Density | 16.69 g/cm³ |
| Melting point | 3017 °C |
| Evaporation | ≈ 3000+ (e-beam) |
| Recommended method | e-beam |
| Packing | Vacuum-sealed foil bag, argon flushed; 1 kg per bag, 25 kg per drum |
| MOQ | 1 kg (samples from 100 g) |
| Lead time | 7–15 working days |
End applications
- Copper diffusion barrier
- High-temperature and corrosion films
- Capacitor and high-k processes
- Optical coatings
- Sputtering target feedstock
Application method
Electron-beam evaporation from a water-cooled copper hearth with a graphite or ceramic liner. Pre-melt slowly to degas the charge and form a stable molten pool before opening the shutter.
Charge weight depends on the liner volume and the fill factor; film consumption depends on area, thickness and utilisation efficiency. Use our crucible fill calculator and film material calculator to size both.
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.





Reviews
There are no reviews yet.