ITO vs AZO vs IGZO: Transparent Conductive Oxide Targets Compared

Transparent conductive oxides all do the same job — conduct electricity while letting light through — but they are not interchangeable. The choice between ITO, AZO and IGZO affects sheet resistance, process temperature, material cost and, in the case of ITO, exposure to indium price swings. This page compares the three on the parameters that usually decide the specification.

Quick comparison

Composition ITO: In2O3 / SnO2 90/10 wt%
AZO: ZnO with 1–2 wt% Al2O3
IGZO: In–Ga–Zn–O, typically 1:1:1 atomic
Typical resistivity ITO 1–3 × 10-4 Ω·cm · AZO 3–10 × 10-4 Ω·cm · IGZO 10-1–100 Ω·cm (semiconductor, not a conductor)
Transparency (visible) ITO > 85% · AZO > 80% · IGZO > 80%
Relative cost ITO high (indium) · AZO low · IGZO medium
Typical process ITO DC or RF, often hot · AZO RF or DC, sometimes H2 anneal · IGZO RF, room temperature
Main use ITO touch panels, displays, solar · AZO low-cost TCO, thin-film PV · IGZO TFT channel layer

When ITO is still the right answer

ITO remains the benchmark for sheet resistance versus transparency. If you need the lowest resistance at a given thickness — touch sensors, OLED cathodes, thin-film solar front contacts — ITO is usually still the specification, and the cost discussion becomes a question of target utilisation and reclaim rather than substitution.

When AZO wins

AZO trades roughly 2–3× higher resistivity for a much lower and more stable material cost, and it avoids indium entirely. It suits thin-film PV, low-cost transparent heaters and buffer layers where 10-3 Ω·cm is acceptable. Note that AZO is sensitive to oxygen content in the sputter gas — small changes shift carrier concentration, so process control matters more than with ITO.

Why IGZO is a different category

IGZO is a semiconductor, not a conductor. It is used as the channel layer in TFT backplanes where high mobility and low off-current matter. It is deposited at low temperature, which is what makes it compatible with flexible substrates — but it is not a replacement for ITO in a transparent electrode.

What we supply

Sizes from 2 inch R&D discs to 300 mm × 300 mm plates, bonded to copper or aluminium backing on request. If you are comparing two materials for a new line, send the target thickness and sheet-resistance requirement and we will quote both.

Frequently asked

Can I use one target chamber for ITO and AZO?

Yes, but cross-contamination matters. Indium residues in an AZO chamber shift the film stoichiometry; most lines keep dedicated cathodes or run a thorough conditioning cycle.

Is AZO as stable as ITO in humidity?

No. AZO films are more sensitive to moisture and to acid attack, so the passivation layer matters more.

Do you supply targets with a specific density?

Yes — ITO is typically supplied at > 99% of theoretical density to limit arcing and particle generation; the density is stated on the certificate.

Related reading: sputtering target specification guide · applications by industry