Indium Gallium Zinc Oxide (IGZO) Sputtering Target

4N (99.99%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

IGZO targets deposit the amorphous oxide semiconductor used as a TFT channel layer. Because the film is a semiconductor rather than a conductor, stoichiometry — not just purity — determines mobility and off-current, and a small cation ratio drift changes device behaviour.

Specification

Composition IGZO (In:Ga:Zn = 1:1:1 at%)
Purity 99.99%
Density 6.4 g/cm³
Melting point ≈1600 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • Cation ratio is the specification: 1:1:1 atomic is standard, other ratios on request.
  • Amorphous as deposited; annealing behaviour depends on the oxygen content of the film.
  • Fine grain and high density reduce nodules on the target surface.

End applications

  • TFT backplanes for displays
  • Flexible electronics
  • Transparent semiconductor layers
  • Sensor and memory devices

Frequently asked

Does the target ratio match the film ratio?

Not exactly — preferential sputtering shifts the film composition slightly. Tell us the film composition you need and we will quote a target ratio that lands there.

Is 1:1:1 the only option?

No. 1:1:1, 1:1:2 and 2:2:1 are all quoted; the choice depends on your carrier mobility target.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Indium Gallium Zinc Oxide (IGZO) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us