Gold targets are used where a film must not oxidise: contacts, infrared reflectors, decorative coatings that have to survive decades, and seed layers that a subsequent process depends on. Because gold is soft and expensive, target utilisation and reclaim matter as much as the sputter rate.
Specification
| Material | Gold (Au) |
|---|---|
| Purity | 4N (99.99%) – 5N (99.999%) |
| Density | 19.30 g/cm³ |
| Melting point | 1064 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing · rotatables on request |
| Grain / texture | Fine grain, controlled texture — stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Soft metal — sputter at low power density to limit nodule formation and target erosion.
- Bonding is strongly recommended above 2 mm thickness; unbonded gold can warp under thermal load.
- Keep the surface free of the silver and copper that often contaminate a shared chamber; a 1% Cu trace changes colour visibly.
End applications
- Semiconductor contacts and seed layers
- IR-reflective and decorative coatings
- Optical filters and beam splitters
- EBL and microelectronics research
Frequently asked
Is 5N gold necessary for decorative work?
No. 4N is indistinguishable visually; 5N matters when the film is an electrical or optical layer where trace metals shift resistivity or absorption.
Can you reclaim used gold targets?
We can quote refining of spent targets against the returned weight; the buy-back value depends on the residual gold content.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.