Purity Grades Explained

3N, 4N, 5N, 6N — What Purity Grade Do You Actually Need?

Buyers often specify “99.99%” because it sounds safe. In practice the right grade depends on which impurities hurt your process, and paying for an extra 9 can double the price without improving the result.

What the “N” notation means

Grade Purity Total impurity Typical use
2N5 99.5% 5,000 ppm Alloying, deoxidisers
3N 99.9% 1,000 ppm General metallurgy, plating
4N 99.99% 100 ppm Battery materials, compounds
5N 99.999% 10 ppm Sputtering targets, electronics
6N 99.9999% 1 ppm Semiconductor, research

The number alone is not enough

Two certificates can both say “99.99%” and describe very different materials, because purity depends on what is being counted and what was measured:

  • Basis: metals basis excludes oxygen and other gases; total basis includes them. A 5N copper on metals basis may contain more oxygen than a 4N5 on total basis.
  • Detection limit: a certificate that reports 99.99% but only measures down to 100 ppm cannot actually prove 4N.
  • Element coverage: harmful impurities differ by application — Fe and Ni for electrical conductivity, O and S for vacuum melting, alkali metals for semiconductor films.

Which grade for which application

Thin-film deposition (sputtering, evaporation)

Use 4N5–5N for most metals. The impurities that matter are those that evaporate or sputter at similar rates to the host metal and end up in the film — typically Fe, Ni, Cr, and for some metals alkali elements. Oxygen content matters more than the headline purity for target density and arc rates.

Battery and precursor materials

4N is usually sufficient for cobalt, nickel and zinc, but specify the individual elements you cannot tolerate (Fe, Cu, Zn cross-contamination in a nickel line, for example) rather than relying on a single purity figure.

Alloying and metallurgy

3N is normally enough for bismuth, tellurium, selenium and copper in alloying, unless the alloy is for a vacuum or electronic application. For free-machining and low-melting alloys, consistency lot to lot matters more than the last 9.

Semiconductor and research

5N–6N with GDMS data. Expect longer lead times, smaller lot sizes, and a price that scales roughly with each additional 9.

How to write the specification

Instead of “99.99% copper”, specify:

Copper, 99.99% min on metals basis.
Fe ≤ 10 ppm, Ni ≤ 10 ppm, Pb ≤ 5 ppm, O ≤ 50 ppm.
Form: ingot, 1 kg pieces. GDMS or ICP-MS report with the lot.

This gives the supplier something testable and gives you something to reject against.

Cost reality

Each additional 9 typically increases price by 30–100% and can double the lead time, because refining beyond 5N moves from electrolytic to zone-refining or vacuum-distillation routes with much lower yield. If your process works at 4N, the 5N premium buys nothing.

Tell us the application and we will recommend the lowest grade that works — and quote the next grade up so you can compare.