Sputtering Targets Guide

Sputtering Targets: How Purity, Density and Grain Size Affect Film Quality

Three targets can carry the same “5N” label and behave completely differently in the chamber. If you are qualifying a supplier, these are the variables that matter.

1. Purity — and which impurities

The headline number is less informative than the impurity table. In practice:

  • Oxygen raises arc rates, creates nodules and particles, and lowers deposition efficiency. For most metals, target-grade material is specified with a maximum oxygen content, not just total purity.
  • Refractory metals (Fe, Ni, Cr, Mo, W) sputter at different rates and can segregate in the film, shifting resistivity and stress.
  • Alkali metals (Na, K, Li) are mobile in oxides and dielectrics — critical for semiconductor and gate-oxide work even at ppm levels.
  • Carbon and sulphur affect film stoichiometry in compound targets.

Ask for GDMS data on the actual target lot, not the raw material lot. Consolidation and bonding can reintroduce contamination.

2. Density and porosity

Target density determines how much material you get per unit volume and how stable the process runs:

Density (% theoretical) Consequence
> 99% Stable, low particle generation, expected for most metals
95–99% Acceptable for many processes; slightly higher arcing
< 95% Open porosity traps gas, outgassing and particles rise, lifetime falls

For metals, density is usually reported against the theoretical value; for oxides and nitrides, the theoretical density assumption varies by phase, so ask which value was used.

3. Grain size and texture

Fine, uniform grain improves film thickness uniformity and reduces “spitting” from preferred-orientation etching. Typical targets are specified in the 20–100 µm range depending on the metal and the deposition mode. If your process is sensitive to uniformity across a large substrate, ask for grain size and texture data, not just a range.

4. Bonding and backing

The target-to-backing-plate bond affects thermal transfer and therefore power density:

  • Elastomer bond — low power, low cost, easy removal
  • Indium bond — higher power density, standard for most metals
  • Diffusion bond — highest power, for demanding processes

Specify the backing plate material and thickness, and whether the target is to be re-bonded at end of life.

5. What to put in the RFQ

Material: copper, 99.999% (5N) min, GDMS report per lot.
Dimensions: Ø 76.2 mm × 6.35 mm thick.
Density: ≥ 99% theoretical.
Oxygen: ≤ 20 ppm.
Bonding: indium to copper backing, 3 mm.
Quantity: 5 pcs, with 2 pcs re-bond option.
Documents: COA + GDMS + packing list.

With this level of detail a supplier can quote a testable product, and you can compare offers on the same basis.

6. Qualifying a new supplier

  1. Order one target and run it against your current supplier’s baseline.
  2. Compare deposition rate, film resistivity/uniformity, particle counts and arc events.
  3. Cut the target after use to inspect grain growth and erosion profile.
  4. Only then negotiate volume — spot prices on 5N material move with the metal, not with the target.

Send your target specification for a quotation →