Toll Processing

Toll Processing

If you need a composition rather than a catalogue grade, we run small heats for qualification and scale to production batches — melting, alloying, atomising and re-melting, with the analysis that proves the result.

Processes

Process Output Typical batch
Vacuum melting / alloying Ingot, button, cast bar 5–200 kg
Atomisation Powder, granule with defined size range 25–500 kg
Re-melting / consolidation Clean ingot from returns or scrap Per lot

Composition control

We work to your composition with tolerances agreed up front, including tramp elements. Each heat is analysed before release: ICP-OES for majors, ICP-MS or GDMS for trace elements, and inert gas fusion where oxygen, nitrogen or hydrogen matter.

Samples and scale-up

New compositions start with a 1–5 kg qualification heat. Once your process accepts it, we hold the recipe and analysis record so subsequent batches match, and can quote production volumes against that baseline.

Material you supply

We also process customer-supplied metal — returns, scrap or off-spec stock — under a toll arrangement, with mass balance and analysis reported back to you.

Send the composition and batch size for a feasibility check →

Scroll to Top