Analytical Services
Independent analysis on your samples or ours, reported in a form your customer or auditor can accept. Useful when qualifying a supplier, checking an incoming lot, or investigating a failed part. Work is carried out by accredited laboratories; our principal partner is Guobiao (Beijing) Testing & Certification Co., Ltd.
Methods and what they answer
| Method | Answers | Sample size |
|---|---|---|
| ICP-OES | Major and minor metal content, ppm level | 1–5 g chips |
| ICP-MS | Trace metals to ppb | 0.5–2 g |
| GDMS | Full trace survey including light elements | 2–5 g |
| Inert gas fusion | O, N, H content | 1 g |
Report contents
- Sample identification and, where relevant, chain of custody
- Method, instrument and detection limits
- Measured values per element, in ppm or %
- Calculated purity on metals or total basis, stated explicitly
- Analyst, reviewer and date
Turnaround
Routine ICP: 3–5 business days. GDMS: 7–10 business days, longer where a full trace survey is requested. Rush service is available at a premium — ask at the time of order.
How to send samples
Send 5–10 g of representative material (chips, granules or a cut section), packed dry, with a description of what the sample is and which elements you care about. We will confirm receipt and the expected report date.