Nickel sheet is the form used when the evaporation source needs a solid charge rather than loose granules — typically a small hearth or a resistance-heated source. Cutting to size avoids the loose packing that causes uneven melting.
Specification
| Material | Nickel (Ni) |
|---|---|
| Purity | 3N5 – 4N5 |
| Melting point | 1455 °C |
| Density | 8.90 g/cm³ |
| Form | Pellets, granules or pieces; custom preforms to drawing |
| Packing | Vacuum-sealed, argon flushed; 1 kg per bag |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Evaporation notes
- Sheet charges melt evenly and are easier to load reproducibly than granules.
- Specify thickness and cut size to match the hearth.
- Nickel is ferromagnetic; keep the sheet flat and away from magnets during handling.
End applications
- Barrier and adhesion layers
- Evaporation feed in sheet-fed sources
- Magnetic film stacks
- Electrode films
Frequently asked
Why use sheet instead of granules?
A solid charge gives a reproducible melt level in a small hearth; granules are better for large liners where filling matters.
Can you cut to my hearth size?
Yes — sheet is supplied cut to drawing, with thickness tolerance stated.
Related reading: e-beam evaporation materials guide · all high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.