Silicon Sputtering Target

3N–6N (99.9–99.9999%)DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Silicon targets cover an unusually wide purity range — 3N to 6N — because the applications are so different: from infrared optical films to semiconductor test structures. Silicon is also the standard material for low-loss IR coatings.

Specification

Material Silicon (Si)
Purity 3N–6N (99.9–99.9999%)
Density 2.33 g/cm³
Melting point 1414 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Silicon is brittle; large targets must be bonded and handled carefully.
  • For IR optics, oxygen content is the limiting factor — silicon oxide absorbs in the 9–11 µm band.
  • Doped silicon targets (B, P, As) are available for specific conductivity requirements.

End applications

  • IR optical coatings and windows
  • Semiconductor test structures and MEMS
  • Thin-film solar and photodetector research
  • Hard, wear-resistant amorphous silicon films

Frequently asked

What purity do I need for IR coatings?

Higher is not always necessary — but oxygen is: SiOx absorption bands matter more than the metal impurity total.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Silicon Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us