Silicon targets cover an unusually wide purity range — 3N to 6N — because the applications are so different: from infrared optical films to semiconductor test structures. Silicon is also the standard material for low-loss IR coatings.
Specification
| Material | Silicon (Si) |
|---|---|
| Purity | 3N–6N (99.9–99.9999%) |
| Density | 2.33 g/cm³ |
| Melting point | 1414 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing |
| Grain / texture | Fine grain; stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Silicon is brittle; large targets must be bonded and handled carefully.
- For IR optics, oxygen content is the limiting factor — silicon oxide absorbs in the 9–11 µm band.
- Doped silicon targets (B, P, As) are available for specific conductivity requirements.
End applications
- IR optical coatings and windows
- Semiconductor test structures and MEMS
- Thin-film solar and photodetector research
- Hard, wear-resistant amorphous silicon films
Frequently asked
What purity do I need for IR coatings?
Higher is not always necessary — but oxygen is: SiOx absorption bands matter more than the metal impurity total.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.