Tantalum is the barrier metal of choice where copper must not migrate and where a film has to survive high temperature. It is dense, hard to machine and expensive, so target utilisation and reclaim weigh on the cost per wafer more than the sputter rate does.
Specification
| Material | Tantalum (Ta) |
|---|---|
| Purity | 3N5 (99.95%) – 4N5 (99.995%) |
| Density | 16.65 g/cm³ |
| Melting point | 3017 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing · rotatables on request |
| Grain / texture | Fine grain, controlled texture — stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Tantalum targets are usually made by vacuum melting or powder metallurgy; the route determines grain size and oxygen content.
- High oxygen gives a resistive beta-phase film — specify gas content for barrier work.
- Bonding is essential for large planar targets; unbonded tantalum cracks under thermal cycling.
End applications
- Diffusion barriers for copper interconnects
- Capacitor and gate electrodes
- Wear and corrosion-resistant coatings
- Implant and medical device coatings
Frequently asked
Alpha or beta phase?
The phase of the deposited film depends on the target and the process; for barrier work you want the low-resistivity alpha phase, which needs low oxygen in the target.
Do you supply tantalum rotatables?
Yes — rotary targets for high-volume lines, quoted against the tool geometry.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.







Reviews
There are no reviews yet.