Indium Sputtering Target

4N–5N (99.99–99.999%)DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Indium targets melt at 157 °C, which makes them the lowest-melting metal in a typical sputtering catalogue. They are used for indium-containing oxide films, for sealing and bonding layers, and as an alloying source — but the low melting point means the target must be bonded and cooled properly or it will simply flow.

Specification

Material Indium (In)
Purity 4N–5N (99.99–99.999%)
Density 7.31 g/cm³
Melting point 156.6 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Low melting point — bond to a water-cooled backing and control the power density.
  • Indium wets many materials; keep a dedicated target if cross-contamination matters.
  • For ITO or IGZO, indium metal is normally alloyed in the target rather than sputtered separately.

End applications

  • Indium-containing oxide films
  • Sealing and bonding layers
  • Alloying source for compound films
  • Cryogenic and vacuum hardware coatings

Frequently asked

Can an indium target be sputtered without bonding?

Not reliably. At 157 °C the metal softens quickly; a bonded, cooled assembly is required for anything beyond very short runs.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Indium Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us