TiAl targets deposit the oxidation-resistant, hard nitride and oxide films used on cutting tools and turbine hardware. Composition control is the whole game: a 2 at% drift in aluminium changes the film hardness and the colour of TiAlN.
Specification
| Material | TiAl (50/50 at%) |
|---|---|
| Purity | TiAl 50/50 at%, ±0.5 wt% |
| Density | 4.0 g/cm³ |
| Melting point | ≈1460 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing |
| Grain / texture | Fine grain; stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Composition tolerance is typically ±0.5 wt% — ask for the assay on the specific lot.
- TiAl is brittle; bonding is standard for anything above 3 mm.
- For TiAlN, nitrogen flow and target composition together set the film stoichiometry.
End applications
- TiAlN hard coatings on cutting tools
- Oxidation-resistant films for turbine components
- Decorative hard coatings
- Aerospace wear protection
Frequently asked
Can you match a specific TiAl composition?
Yes — 50/50 at% is standard, but 48/52 and 60/40 are common variants. Specify the atomic ratio and we quote against it.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.