CoFeB Alloy Sputtering Target

CoFeB 60/20/20 at%, ±0.5 wt%DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

CoFeB targets deposit the free layer in magnetic tunnel junctions, where a fraction of a percent of boron changes the crystallisation temperature and therefore the device performance. Composition is the specification.

Specification

Material CoFeB (60/20/20 at%)
Purity CoFeB 60/20/20 at%, ±0.5 wt%
Density ≈8.2 g/cm³
Melting point ≈1200 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Boron content is the critical parameter — ±0.5 at% is tight for a reason.
  • Amorphous as deposited; annealing behaviour depends on the boron level.
  • Store sealed — boron-containing alloys are sensitive to moisture.

End applications

  • Magnetic tunnel junctions in MRAM
  • Spin-transfer torque devices
  • Magnetic sensors
  • Spintronics research

Frequently asked

How do you verify boron content?

By ICP or GDMS depending on the level required; the certificate states the method and the measured composition.

Why does boron content matter so much?

Boron controls when the CoFeB layer crystallises during anneal. A drift of a few tenths of an atomic percent moves that temperature and changes the tunnel magnetoresistance.

How should CoFeB be stored?

Vacuum packed, cool and dry. Moisture and oxygen affect the as-deposited state.

Can you supply a matched set of magnetic layers?

Yes — CoFeB, NiFe and Co targets can come from the same production batch so the stack composition tracks.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “CoFeB Alloy Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us