Tungsten-Titanium (WTi) Sputtering Target

W/Ti 90/10 wt%, ±0.5 wt%DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

WTi (TiW) targets deposit the barrier layer that has separated aluminium from silicon for decades, and they remain the standard for contacts and via liners in mature nodes. The alloy is refractory and brittle — density and bonding decide whether the target survives.

Specification

Material W/Ti (90/10 wt%)
Purity W/Ti 90/10 wt%, ±0.5 wt%
Density ≈18.7 g/cm³
Melting point ≈3300 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Very brittle — bonding is mandatory and handling damage is a real risk.
  • Nitrogen addition (WTiN) improves barrier performance; specify if the process needs it.
  • Density above 99% limits the particles that cause via failures.

End applications

  • Diffusion barriers for Al and Cu metallisation
  • Contact and via liners
  • Hard, wear-resistant coatings
  • X-ray and radiation shielding films

Frequently asked

Why is WTi so brittle?

The tungsten–titanium intermetallic phase is hard and brittle. Targets are made by powder metallurgy or hot pressing and must be bonded before use.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Tungsten-Titanium (WTi) Sputtering Target”

Your email address will not be published. Required fields are marked *