Chromium Sputtering Target

3N–4N5 (99.9–99.995%)DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Chromium targets are among the most widely used of all: adhesion layers under gold, hard decorative coatings, and the bonding layer in Cr/Ni/Au stacks. Chromium is also a strong oxygen getter, so the target surface state matters more than for a noble metal.

Specification

Material Chromium (Cr)
Purity 3N–4N5 (99.9–99.995%)
Density 7.19 g/cm³
Melting point 1907 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Chromium forms a passive oxide that is hard to remove in situ; a pre-sputter step is usually needed.
  • Nodules and arcing are common — fine grain and high density reduce both.
  • For decorative coatings, nitrogen addition (CrN) changes colour and hardness.

End applications

  • Adhesion layers in Cr/Ni/Au metallisation
  • Decorative and wear-resistant CrN coatings
  • Optical and reflective films
  • Mold and tool coatings

Frequently asked

Why does my chromium film peel?

Usually an oxidised target surface or insufficient substrate heating. Pre-sputter longer and check the base pressure before opening the shutter.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Chromium Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us