Manganese Sputtering Target

3N–4N (99.9–99.99%)DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Manganese targets are used in magnetic and antiferromagnetic stacks, in manganese-containing oxides and as an alloying element in steel-facing coatings. Manganese oxidises aggressively, which makes target handling and chamber cleanliness the deciding factors.

Specification

Material Manganese (Mn)
Purity 3N–4N (99.9–99.99%)
Density 7.21 g/cm³
Melting point 1246 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Strong oxygen getter — store sealed and pre-sputter thoroughly.
  • Manganese is brittle; large planar targets should be bonded.
  • In antiferromagnetic stacks (IrMn, PtMn) manganese is usually sputtered as part of an alloy target.

End applications

  • Antiferromagnetic layers in magnetic devices
  • Manganese oxide films
  • Alloying component in corrosion-resistant coatings
  • Battery cathode research

Frequently asked

Is manganese hazardous to handle?

Manganese dust and fume are regulated in most jurisdictions. Targets are supplied as solid, machined pieces; follow your EHS rules for the sputter process.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Manganese Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us