Tin Sputtering Target

4N–5N (99.99–99.999%)DiscMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Tin targets are used for solderable layers, for transparent oxide research and as an alloying component in Sn-based films. Like zinc and indium, tin melts low — at 232 °C — so the process window sits between “not hot enough to sputter well” and “hot enough to melt the target”.

Specification

Material Tin (Sn)
Purity 4N–5N (99.99–99.999%)
Density 7.28 g/cm³
Melting point 232 °C
Form Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing
Grain / texture Fine grain; stated on request
Bonding Indium or elastomer to Cu / Al backing, bond coverage checked
Packing Vacuum-sealed, foam-lined case with flatness record
MOQ 1 pc
Lead time 15–25 working days

Sputtering notes

  • Low melting point — bonding and power control are both essential.
  • Tin grows whiskers under stress; films intended for electronics need a cap layer.
  • For solderable finishes, a SnAg or SnCu alloy target often outperforms pure tin.

End applications

  • Solderable surface finishes
  • Tin oxide and transparent conductor research
  • Corrosion-resistant coatings
  • Alloy films for electronic assembly

Frequently asked

Why use a SnAg target instead of pure tin?

Whisker growth and melting behaviour. Alloyed films are more stable under thermal cycling, which matters for connectors and PCB finishes.

Related reading: target specification guide · all metal sputtering targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Tin Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us