Permalloy targets deposit the soft magnetic films used for shielding and for flux guides in sensors. The 80/20 composition is chosen for near-zero magnetostriction and high permeability — both of which drift if the ratio moves.
Specification
| Material | Ni/Fe (80/20 wt%) |
|---|---|
| Purity | Ni/Fe 80/20 wt%, ±0.5 wt% |
| Density | ≈8.7 g/cm³ |
| Melting point | ≈1450 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing |
| Grain / texture | Fine grain; stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Composition control matters more than purity: 81/19 behaves differently from 79/21.
- Soft magnetic — thin films are sensitive to stress, so sputter rate and pressure both matter.
- Bonding recommended for targets above 3 mm.
End applications
- Magnetic shielding films
- Flux guides in sensors and heads
- Soft magnetic underlayers
- MEMS magnetic components
Frequently asked
Do you supply other NiFe ratios?
Yes — 45/55 and 20/80 are also common for specific applications. Specify the ratio and whether wt% or at%.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.