Indium for ITO Targets: Purity, Form and What to Specify
Indium is one of the few metals where the gap between 4N and 5N changes the economics of the whole process — because the target, not the metal, is where the money sits. Here is what actually matters when buying indium for ITO.
Why ITO drives the specification
Indium tin oxide targets are usually made by mixing In₂O₃ and SnO₂ powders, pressing and sintering. That means the impurities in the indium follow through the oxide and into the target. Elements that do not volatilise during sintering stay; elements that do, leave — which is why the impurity list matters more than the headline number.
Purity: 4N, 4N5 or 5N
- 4N (99.99%) — adequate for many display-grade ITO targets, provided the certificate states the impurity table
- 4N5–5N — standard for targets used in high-end displays and touch panels, where film resistivity and transmittance targets are tight
- 5N+ — required for some semiconductor and optical coatings; the premium is real and should be justified by your process data
Ask for GDMS on the indium lot if you are qualifying 5N. ICP-OES alone cannot prove 5N.
Form
Indium is soft and low-melting (156.6 °C), so form affects handling more than for other metals:
- Ingot (1 kg or 5 kg) — cut and weighed in a clean room, then vacuum-sealed; standard for target makers
- Shot / granule — convenient for small melts and alloying, higher surface area so packaging matters more
- Rod / wire — for sealing and bonding applications rather than target production
What to put in the RFQ
Indium, 99.995% min, metals basis.
Fe ≤ 5 ppm, Cu ≤ 3 ppm, Pb ≤ 5 ppm, Cd ≤ 2 ppm, Tl ≤ 2 ppm.
Form: 1 kg ingots, vacuum-sealed foil bags, 25 kg per drum.
GDMS report per lot. Quantity 200 kg, delivery FOB Shanghai.
A common mistake
Buying on price per kilogram alone. Indium’s price moves, but the cost of a failed target batch — lost powder, lost sintering run, lost customer qualification — is far larger than a few percent on the metal. Qualify the lot, keep the certificate, and only then negotiate volume.
Request an indium quotation with the purity basis you need →