Cobalt Evaporation Granules 3N5-5N

Co3N5–5N (99.95–99.999%)GranulesMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Cobalt evaporates at a moderate temperature and is used mainly for magnetic films and as an alloy component. Granules are the practical form for e-beam charges because they fill the liner evenly and can be topped up.

Specification

Material Cobalt (Co)
Purity 3N5 – 5N
Melting point 1495 °C
Density 8.90 g/cm³
Form Pellets, granules or pieces; custom preforms to drawing
Packing Vacuum-sealed, argon flushed; 1 kg per bag
MOQ 100 g (samples from 10 g)
Lead time 10–20 working days

Evaporation notes

  • Ferromagnetic — the charge can disturb the beam sweep on some sources.
  • Cobalt oxidises slowly; sealed storage keeps first-melt behaviour repeatable.
  • For magnetic stacks, order the same lot as the partner layers.

End applications

  • Magnetic film stacks
  • Hard and wear-resistant coatings
  • Alloy component for CoFe and CoCr
  • Battery and catalyst research

Frequently asked

Granules or pellets for cobalt?

Granules fill a liner more densely and are easier to top up mid-run; pellets give a more repeatable melt level.

Is 5N cobalt available?

Yes, up to 5N with a GDASS/ICP certificate, quoted on request.

Related reading: e-beam evaporation materials guide · all high-purity evaporation materials

Related resources

Reviews

There are no reviews yet.

Be the first to review “Cobalt Evaporation Granules 3N5-5N”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us