The high-purity grade of our cobalt evaporation granules: the same material as the standard granules, but supplied against a tighter certificate for magnetic and semiconductor work where trace iron and nickel shift the film behaviour.
Specification
| Material | Cobalt (Co) |
|---|---|
| Purity | 3N5 – 5N |
| Melting point | 1495 °C |
| Density | 8.90 g/cm³ |
| Form | Pellets, granules or pieces; custom preforms to drawing |
| Packing | Vacuum-sealed, argon flushed; 1 kg per bag |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Evaporation notes
- Certificate states iron, nickel and oxygen individually — ask for the figures.
- Ferromagnetic; a compensated source gives a more uniform melt.
- Vacuum packed with desiccant; use promptly after opening.
End applications
- Magnetic tunnel junction layers
- Semiconductor cobalt liners
- Precision magnetic stacks
- Research films
Frequently asked
What is different from standard cobalt granules?
The certificate: tighter limits on iron, nickel and oxygen, verified per lot. The material is the same element.
Do you supply both forms?
Yes — standard and high-purity cobalt granules are separate products; pick the one your specification calls for.
Related reading: e-beam evaporation materials guide · all high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.