Gallium oxide is an ultra-wide-bandgap semiconductor being developed for power devices and solar-blind UV photodetectors. Targets must be phase-pure (beta phase is the stable one) and dense, because film quality determines the device.
Specification
| Composition | Ga2O3 |
|---|---|
| Purity | 99.9–99.99% |
| Density | 5.88 g/cm³ |
| Melting point | 1725 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- Beta phase is the stable polymorph — specify phase purity.
- Wide band gap means the film is transparent deep into the UV.
- Gallium is expensive; utilisation and reclaim matter.
End applications
- Power device research
- Solar-blind UV photodetectors
- Transparent conductive oxide alternatives
- Phosphor and catalyst films
Frequently asked
Which phase do you supply?
Beta-Ga2O3 is standard; alpha phase is available on request for specific epitaxy work.
Can Ga2O3 be doped?
Yes — Sn-doped and Si-doped targets are quoted for n-type conductivity work.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.