Vanadium targets are used for vanadium oxide films (VO2 thermochromics, V2O5 electrochromics), for nitride hard coatings and as an alloying element in TiAlV systems. Vanadium is a strong getter and its oxides are volatile at process temperature, so target purity and chamber cleanliness interact.
Specification
| Material | Vanadium (V) |
|---|---|
| Purity | 3N–4N (99.9–99.99%) |
| Density | 6.11 g/cm³ |
| Melting point | 1910 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing |
| Grain / texture | Fine grain; stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Vanadium oxides are volatile at elevated temperature — keep the substrate temperature modest.
- For VO2 the oxygen partial pressure, not the target, controls the phase; reactive sputtering from a metal target is normal.
- Vanadium is ductile but work-hardens quickly; machined surfaces are stable if protected.
End applications
- VO2 thermochromic and V2O5 electrochromic films
- VN and VCN hard coatings
- Alloying feedstock for TiAlV
- Catalyst and electrode films
Frequently asked
Why is VO2 so sensitive to process?
The thermochromic phase exists in a narrow oxygen window; a small change in the O2 flow shifts the transition temperature.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews