Tungsten targets serve two very different jobs: a thin diffusion barrier in a semiconductor stack, and a hard, wear-resistant coating on a tool. The two need different specifications, and the split is usually density and gas content rather than purity.
Specification
| Material | Tungsten (W) |
|---|---|
| Purity | 3N5 (99.95%) · 4N on request |
| Density | 19.25 g/cm³ |
| Melting point | 3422 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″, 12″ · rectangular plates to drawing · rotatables on request |
| Grain / texture | Fine grain, controlled texture — stated on request |
| Bonding | Indium or elastomer to Cu / Al backing, bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with flatness record |
| MOQ | 1 pc |
| Lead time | 15–25 working days |
Sputtering notes
- Density above 99% of theoretical limits porosity and particle generation.
- Oxygen and nitrogen cause film resistivity to climb; ask for the gas figures.
- Tungsten is brittle — large planar targets must be bonded, and handling damage is a real risk.
End applications
- Diffusion barriers in semiconductor stacks
- Hard and wear-resistant coatings
- Electrodes and contact layers
- X-ray and radiation shielding films
Frequently asked
Why does my tungsten film have high resistivity?
Usually oxygen or nitrogen in the target, or a low-density target that sputters unevenly.
Can tungsten be sputtered from a rotatable?
Yes, for high-volume barrier lines; the geometry is quoted to the tool.
Related reading: target specification guide · all metal sputtering targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.