Gold-Germanium-Nickel (AuGeNi) Evaporation Pellets

4N (99.99%)PelletsMelting

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

AuGeNi is the standard ohmic contact metallisation for n-GaAs and GaN devices. The eutectic composition melts at about 361 °C and wets the semiconductor cleanly, which is why it has survived every attempt to replace it.

Specification

Material Au/Ge/Ni 88/12/1 wt%
Purity 99.99%
Melting point ≈361 (eutectic) °C
Form Pellets, granules or pieces; custom preforms to drawing
Packing Vacuum-sealed, argon flushed; 1 kg per bag
MOQ 100 g (samples from 10 g)
Lead time 10–20 working days

Evaporation notes

  • Composition is the specification — 88/12/1 wt% with nickel at about 1%.
  • Pre-melt and degas: germanium oxidises easily and a poor melt gives a non-ohmic contact.
  • Store sealed; the alloy is not hazardous but germanium oxide changes behaviour.

End applications

  • Ohmic contacts to n-GaAs and GaN
  • Compound semiconductor metallisation
  • Die attach and wafer bonding
  • Optoelectronic devices

Frequently asked

Why is nickel added to AuGe?

Nickel improves wettability and contact morphology; without it the contact tends to ball up.

Do you supply custom AuGeNi ratios?

Yes — composition is verified per lot and can be adjusted to your process.

Related reading: e-beam evaporation materials guide · all high-purity evaporation materials

Related resources

Reviews

There are no reviews yet.

Be the first to review “Gold-Germanium-Nickel (AuGeNi) Evaporation Pellets”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us