AuGeNi is the standard ohmic contact metallisation for n-GaAs and GaN devices. The eutectic composition melts at about 361 °C and wets the semiconductor cleanly, which is why it has survived every attempt to replace it.
Specification
| Material | Au/Ge/Ni 88/12/1 wt% |
|---|---|
| Purity | 99.99% |
| Melting point | ≈361 (eutectic) °C |
| Form | Pellets, granules or pieces; custom preforms to drawing |
| Packing | Vacuum-sealed, argon flushed; 1 kg per bag |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Evaporation notes
- Composition is the specification — 88/12/1 wt% with nickel at about 1%.
- Pre-melt and degas: germanium oxidises easily and a poor melt gives a non-ohmic contact.
- Store sealed; the alloy is not hazardous but germanium oxide changes behaviour.
End applications
- Ohmic contacts to n-GaAs and GaN
- Compound semiconductor metallisation
- Die attach and wafer bonding
- Optoelectronic devices
Frequently asked
Why is nickel added to AuGe?
Nickel improves wettability and contact morphology; without it the contact tends to ball up.
Do you supply custom AuGeNi ratios?
Yes — composition is verified per lot and can be adjusted to your process.
Related reading: e-beam evaporation materials guide · all high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.