AuSn 80/20 is the eutectic gold-tin alloy used for flux-free die attach and for deposited solder layers. It melts sharply at 280 °C with no pasty range, which gives a predictable joint and no flux residue inside a hermetic package.
Specification
| Material | Au/Sn 80/20 wt% |
|---|---|
| Purity | 99.99% |
| Melting point | 280 (eutectic) °C |
| Form | Pellets, granules or pieces; custom preforms to drawing |
| Packing | Vacuum-sealed, argon flushed; 1 kg per bag |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Evaporation notes
- Eutectic composition means a single melting point — no pasty range.
- Tin oxidises; vacuum packing and prompt use keep the wet-out consistent.
- For preforms rather than evaporation, see our AuSn preform page.
End applications
- Flux-free die attach for laser diodes and LEDs
- Hermetic package sealing
- Deposited solder layers
- Optoelectronic module assembly
Frequently asked
Can AuSn be evaporated without flux?
Yes, provided the surfaces are gold or nickel-gold and the atmosphere is clean.
Do you supply AuSn as preforms?
Yes — preforms are cut to drawing; this page covers the evaporation pellets.
Related reading: e-beam evaporation materials guide · all high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.