Tungsten sheet at 3N5 purity from 0.2 mm to 5.0 mm, cut to size. Used for heat shields, evaporation boats and electrodes where the operating temperature rules out every other metal.
Specification
| Metal | Tungsten (W) |
|---|---|
| Purity | 3N5 (99.95%) |
| Form | Sheet |
| Dimensions | Thickness 0.2–5.0 mm; width up to 200 mm; cut to size |
| Density | 19.25 g/cm³ |
| Melting point | 3422 °C |
| Packing | Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case |
| MOQ | By agreement — quoted per order |
| Lead time | 10–20 working days |
Tolerances and handling
- Tungsten sheet is brittle; specify the grain direction and avoid sharp internal corners in the design.
- For evaporation boats, the surface finish affects wetting — a polished boat behaves differently from a rolled one.
- Cut edges should be deburred; a burr becomes a crack initiation site under thermal cycling.
End applications
- Heat shields and radiation baffles
- Evaporation boats and liners
- Electrodes and sputter shielding
- High-temperature tooling
Frequently asked
Can tungsten sheet be formed?
Only at high temperature. Cold forming cracks it; most parts are machined or ground from plate.
Do you supply tungsten boats?
We supply sheet and can quote boats to drawing; standard boats are also available.
Related reading: all wire, foil and solder products · high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.