How to Read a Certificate of Analysis (and What to Reject)
A COA is a legal document in most purchase contracts, but a surprising number are unusable: no method, no detection limits, no lot number, or a purity figure that cannot be reproduced. Here is how to read one in two minutes.
The five things every COA must contain
- Lot number that matches the drum label and the packing list
- Material and form — “copper ingot” is not enough; state grade and dimensions
- Purity basis — metals basis or total basis, and what is excluded
- Impurity table with values and detection limits per element
- Method and date — ICP-OES, ICP-MS, GDMS, inert gas fusion; test date and signatory
Reading the impurity table
Compare what is reported against what your process cares about. A COA for 5N copper that lists only Fe, Ni and Pb is not a full trace survey — it is a targeted one. For sputtering targets, oxygen is usually the number that matters most; if it is missing, ask for it.
| What you see | What it means |
|---|---|
| Values reported as “< 10 ppm” | Detection limit is 10 ppm — the method cannot prove 5N |
| “99.99% min” with no table | Untestable; treat as a marketing claim |
| Metals basis stated, oxygen absent | Gases are excluded by definition — ask for the gas analysis separately |
| Same values copied across lots | Possibly a template; ask for the raw instrument output |
Signature, date and laboratory
The report should identify the laboratory and the analyst, and carry a date that is before the packing date. A COA dated after shipment, or issued by a trading company rather than a laboratory, deserves a follow-up question.
When to reject
- Lot number does not match the drum
- Purity basis is not stated
- The method cannot reach the claimed purity
- No detection limits
- Values are identical across multiple lots and dates
Rejecting on paperwork is cheaper than rejecting after the material is in your furnace. If a supplier cannot produce a compliant COA before shipment, that is itself information about the supplier.
See how we document our own lots → or request a sample COA with your quotation.