High-purity copper wire at 5N (99.999%), from 0.1 mm to 3.0 mm, supplied on spools. Used where conductivity and low oxygen content both matter — semiconductor interconnects, evaporation feed and precision contacts.
Specification
| Metal | Copper (Cu) |
|---|---|
| Purity | 5N (99.999%) |
| Form | Wire |
| Dimensions | Ø 0.1–3.0 mm; spools of 100 g–1 kg |
| Density | 8.96 g/cm³ |
| Melting point | 1085 °C |
| Packing | Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case |
| MOQ | By agreement — quoted per order |
| Lead time | 10–20 working days |
Tolerances and handling
- Oxygen, not trace metals, is the limiting impurity for conductivity; ask for the figure.
- Wire above 1 mm is supplied in coils rather than on spools.
- Copper tarnishes — sealed packing and a defined shelf life apply.
End applications
- Interconnects and bonding wire
- Evaporation feed for copper films
- High-conductivity contacts
- Analytical standards
Frequently asked
Is 5N copper oxygen-free?
It is low-oxygen by specification; the exact figure is stated on the certificate. If you need OFC-grade, tell us the limit.
Do you supply 0.05 mm copper wire?
0.1 mm is our standard minimum; finer sizes can be quoted.
Related reading: all wire, foil and solder products · high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.