Tin foil at 4N purity from 0.02 mm, for soldering, tinning and evaporation. Tin is soft and low-melting (232 °C), which makes foil the practical form for covering or interleaving surfaces that must be joined later.
Specification
| Metal | Tin (Sn) |
|---|---|
| Purity | 4N (99.99%) |
| Form | Foil |
| Dimensions | Thickness 0.02–0.5 mm; width 10–200 mm |
| Density | 7.28 g/cm³ |
| Melting point | 232 °C |
| Packing | Vacuum-sealed, argon flushed; spool or flat pack in a foam-lined case |
| MOQ | By agreement — quoted per order |
| Lead time | 10–20 working days |
Tolerances and handling
- Tin foil grows whiskers under stress — for electronics, choose a SnAg or SnCu alloy instead of pure tin.
- Tin is soft and creases easily; flat packing only.
- Store cool: tin transforms slowly at low temperature (tin pest), which is why shelf life is defined.
End applications
- Soldering and tinning
- Battery and capacitor foils
- Evaporation and sputtering feedstock
- Corrosion-test coupons
Frequently asked
Does pure tin foil grow whiskers?
Yes, under compressive stress. For electronics, alloyed tin (SnAgCu) or a nickel barrier avoids the problem.
What purity is standard?
4N (99.99%); 5N is available on request for semiconductor work.
Related reading: all wire, foil and solder products · high-purity evaporation materials
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.