Chromium is the standard adhesion layer under gold and the standard hard decorative layer on its own. It is a strong getter, so the first melt releases gas and the film quality depends on how patiently the charge is degassed.
Specification
| Material | Chromium (Cr) |
|---|---|
| Purity | 3N5 – 4N5 |
| Melting point | 1907 °C |
| Density | 7.19 g/cm³ |
| Form | Pellets, granules or pieces; custom preforms to drawing |
| Packing | Vacuum-sealed, argon flushed; 1 kg per bag |
| MOQ | 100 g (samples from 10 g) |
| Lead time | 10–20 working days |
Evaporation notes
- Pre-melt slowly — chromium absorbs oxygen and spits if heated fast.
- Granules fill the liner densely, giving a stable melt level and less bridging than chunks.
- For decorative work, nitrogen addition (CrN) changes colour and hardness.
End applications
- Adhesion layers in Cr/Ni/Au stacks
- Decorative and wear-resistant coatings
- Optical and reflective films
- Mould and tool coatings
Frequently asked
Why does my chromium film peel?
An oxidised target surface or insufficient degassing. Pre-sputter or pre-melt longer and check the base pressure.
Granules or pieces — which is better?
Granules give a more even melt and are easier to top up; pieces are cheaper per kilogram for large charges.
Supplied to a Beijing semiconductor equipment maker at roughly 8 tonnes per year — see the supply case.
Related reading: e-beam evaporation materials guide · all high-purity evaporation materials
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.