Molybdenum Dioxide (MoO₂) Sputtering Target

3N (99.9%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Molybdenum dioxide is used as an electrode and catalyst material, and as a component in lithium battery and supercapacitor research. It decomposes rather than melting cleanly, so target density and bonding decide whether it survives a run.

Specification

Composition MoO2
Purity 99.9%
Density 6.47 g/cm³
Melting point ≈1100 (decomposes) °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • MoO2 decomposes before melting — thermal management is critical.
  • Density above 95% is typical; porosity shows as particles.
  • For battery work, the film phase and nanostructure matter more than purity.

End applications

  • Electrode and catalyst films
  • Lithium battery and supercapacitor research
  • Gas sensors
  • Optical absorber layers

Frequently asked

Why does my MoO2 target crack?

Thermal stress from poor bonding or a fast ramp. The material decomposes rather than melting, so the target cannot redistribute heat by melting.

Do you supply MoO3 as well?

MoO3 is a separate product used as a hole-injection layer; both are available.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Molybdenum Dioxide (MoO₂) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us