Niobium pentoxide offers a higher index than Ta2O5 at lower cost, which makes it attractive for NIR filters and for high-index layers where laser damage is not the limiting requirement.
Specification
| Composition | Nb2O5 |
|---|---|
| Purity | 99.9–99.99% |
| Density | 4.60 g/cm³ |
| Melting point | 1520 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- Higher index than Ta2O5 but slightly more absorbing in the UV.
- Stoichiometry affects both index and absorption — specify for optical work.
- Density above 97% is normal; lower density shows as scatter.
End applications
- NIR and IR optical filters
- High-index layers in AR stacks
- Electrochromic films
- Dielectric layers
Frequently asked
Is Nb2O5 a drop-in replacement for Ta2O5?
In many NIR designs yes, with a re-optimised stack. In the UV, absorption is higher.
What purity do you supply?
3N–4N depending on grade; the certificate states the level.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.