Bismuth Oxide (Bi₂O₃) Sputtering Target

3N (99.9%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Bismuth oxide has an unusually high refractive index for a low-melting oxide, which makes it useful in optical coatings and in visible-light photocatalysis. Its low melting point (824 °C) means the target must be cooled and sputtered gently.

Specification

Composition Bi2O3
Purity 99.9%
Density 8.90 g/cm³
Melting point 824 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • Low melting point — bond the target and keep power density down.
  • High index makes it attractive for optical designs, but films can be oxygen-deficient.
  • Bismuth is a heavy element; sputter yield is low compared with light oxides.

End applications

  • Optical coatings and high-index layers
  • Photocatalytic films
  • Solid oxide and sensor research
  • Decorative and iridescent coatings

Frequently asked

Why does my Bi2O3 film look metallic?

Oxygen deficiency. Bi2O3 reduces easily; increase the oxygen partial pressure or use a fully stoichiometric target.

Can Bi2O3 be sputtered without bonding?

Not reliably. At 824 °C the target softens quickly; a bonded, cooled assembly is required.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Bismuth Oxide (Bi₂O₃) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top