Zirconium dioxide is used as a tough, high-index layer that survives thermal cycling better than TiO2, and as a thermal barrier in coated tooling. Its high melting point makes the target hard to densify, so density is the value to check.
Specification
| Composition | ZrO2 |
|---|---|
| Purity | 99.9–99.99% |
| Density | 5.68 g/cm³ |
| Melting point | 2715 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- High melting point makes full densification difficult — ask for the density figure.
- ZrO2 can exist in monoclinic, tetragonal or cubic phase; the phase affects film stress.
- For tool coatings, yttria-stabilised zirconia is often preferred.
End applications
- Laser and optical coatings
- Thermal barrier layers
- Wear-resistant tool coatings
- Solid oxide fuel cell research
Frequently asked
Why is ZrO2 density often lower than other oxides?
The high melting point limits sintering. Dense targets need hot pressing or sintering aids, and the density should be stated.
Do you supply yttria-stabilised zirconia?
Yes — YSZ targets are quoted to the yttria content you specify.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.





Reviews
There are no reviews yet.