Silicon monoxide is used mainly as an evaporation material for optical and protective coatings, and as a sputtering target where a sub-stoichiometric silicon oxide film is wanted. Its low density and reactivity make dense targets difficult to produce.

Specification

Composition SiO
Purity 99.9%
Density 2.13 g/cm³
Melting point 1702 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • SiO is reactive and disproportionates at temperature — handle and store sealed.
  • For optical coatings, the film index depends on the oxygen content.
  • Density is lower than SiO2; targets are fragile.

End applications

  • Optical coatings with tuned index
  • Protective and release layers
  • Evaporation source for SiO films
  • Barrier layers in packaging

Frequently asked

SiO target or SiO evaporation pellets?

For thin optical films, evaporation is more common; for large-area sputtering a target is used. Both are available.

Why is the film index inconsistent?

SiO disproportionates into Si and SiO2 during heating, so the film composition depends on the source history.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Silicon Monoxide (SiO) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us