Silicon Dioxide (SiO₂) Sputtering Target

3N–4N (99.9–99.99%)DiscSintering

Request a Quote for this Product

Include quantity, dimensions and destination — we reply within one business day.

Assay certificate with every lotVacuum / argon packagingExport documents preparedQuote within 1 business day

Silicon dioxide is the standard low-index layer in optical coatings and the standard insulator in thin-film electronics. It is also the material that most often exposes a process problem, because a slightly oxygen-deficient SiO2 film absorbs in the UV and shifts the coating design.

Specification

Composition SiO2
Purity 99.9–99.99%
Density 2.65 g/cm³
Melting point 1710 °C
Form Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request
Bonding Indium or elastomer to Cu backing; bond coverage checked
Packing Vacuum-sealed, foam-lined case with density and stoichiometry report
MOQ 1 pc
Lead time 20–30 working days

What decides the film

  • Stoichiometry matters: SiOx with x below 2 absorbs in the UV.
  • SiO2 targets are insulators — RF sputtering, with the target bonded for cooling.
  • For thick layers, deposition rate is low; consider a rotatable for volume work.

End applications

  • Low-index layers in optical filters
  • Insulating layers in thin-film electronics
  • Protective and passivation coatings
  • Planarisation layers

Frequently asked

Can SiO2 be sputtered with DC?

No — it is an insulator. RF (or pulsed DC with a special arrangement) is required.

Why does my SiO2 film absorb?

Oxygen deficiency or contamination. Check the target stoichiometry and the base pressure.

Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets

Related resources

Reviews

There are no reviews yet.

Be the first to review “Silicon Dioxide (SiO₂) Sputtering Target”

Your email address will not be published. Required fields are marked *

Scroll to Top
Chat with us