Tin dioxide targets are used for gas sensors, for transparent conductors in some architectures and as a component of ITO replacements. SnO2 sublimes rather than melting cleanly, which makes target density and thermal bonding unusually important.
Specification
| Composition | SnO2 |
|---|---|
| Purity | 99.9–99.99% |
| Density | 6.95 g/cm³ |
| Melting point | 1630 (sublimes) °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- SnO2 sublimes — a poorly bonded target will crack from thermal gradients before it wears out.
- Density above 98% limits the particle generation that ruins sensor films.
- For gas sensors, dopants (Pd, Sb) are usually added; specify the level.
End applications
- Gas sensors (CO, NOx, ethanol)
- Transparent conductive layers
- Catalyst supports
- Varistor and ceramic electronics
Frequently asked
Why does my SnO2 target crack?
Thermal stress from poor bonding or too-aggressive power ramp. SnO2 does not conduct heat well, so the bond and the ramp rate both matter.
Do you supply doped SnO2?
Yes — Sb-doped and Pd-doped targets are quoted to specification.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.






Reviews
There are no reviews yet.