Cuprous oxide is a p-type semiconductor with a direct band gap near 2.1 eV, which makes it interesting for solar cells, photodetectors and transparent electronics. It is a different material from CuO, and the target phase decides which film you get.
Specification
| Composition | Cu2O (cuprous) |
|---|---|
| Purity | 99.9% |
| Density | 6.0 g/cm³ |
| Melting point | 1235 °C |
| Form | Discs 2″, 3″, 4″, 6″, 8″ · plates to drawing · rotatables on request |
| Bonding | Indium or elastomer to Cu backing; bond coverage checked |
| Packing | Vacuum-sealed, foam-lined case with density and stoichiometry report |
| MOQ | 1 pc |
| Lead time | 20–30 working days |
What decides the film
- Cu2O and CuO are different targets — specify the phase.
- Cu2O is metastable; deposition conditions can oxidise it further to CuO.
- For solar work, the carrier mobility depends strongly on film quality.
End applications
- p-type solar cell absorbers
- Photodetectors
- Transparent semiconductor research
- Gas sensors
Frequently asked
How do I keep the film as Cu2O rather than CuO?
Control the oxygen partial pressure and the substrate temperature; too much oxygen gives CuO. Start from a phase-pure Cu2O target.
Is Cu2O available in production quantities?
Yes, but it is mainly a research and sensor material rather than a high-volume coating.
Related reading: targets for optical coatings · ITO vs AZO vs IGZO · all ceramic targets
Related resources
- Applications — where this material is used, by industry.
- Deposition methods — e-beam vs thermal, liner choice, pre-melt and defect fixes.
- Crucible fill calculator — how much charge fits in the liner.
- Film material calculator — material needed for a given thickness.